• ASTM A213/A213M-01a

ASTM A213/A213M-01a

Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

ASTM International, 09/10/2001

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:10/09/2001

Pages:9

File Size:1 file , 75 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers minimum-wall-thickness, seamless ferritic and austenitic steel, boiler and superheater tubes and austenitic steel heat-exchanger tubes, designated Grades T5, TP304, etc. These steels are listed in Tables 1.

1.2 Grades S30432, TP304H, TP309H, TP309HCb, TP310H, TP310HCb, TP310HCbN, TP316H, TP321H, TP347H, TP347HFG (fine grained) and TP348H are modifications of Grades TP304, TP309S, TP309Cb, TP310S, TP310Cb, TP316, TP321, TP347, and TP348, and are intended for high-temperature service, such as for superheaters and reheaters.

1.3 The tubing sizes and thicknesses usually furnished to this specification are 1/8 in. [3.2 mm] in inside diameter to 5 in. [127 mm] in outside diameter and 0.015 to 0.500 in. [0.4 to 12.7 mm], inclusive, in minimum wall thickness. Tubing having other dimensions may be furnished, provided such tubes comply with all other requirements of this specification.

1.4 Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] in inside diameter or 0.015 in. [0.4 mm] in thickness.

1.5 Optional supplementary requirements are provided and, when desired, shall be so stated in the order.

1.6 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification. The inch-pound units shall apply unless the "M" designation of this specification is specified in the order.

More ASTM standard pdf

ASTM D6405-99(2004)

ASTM D6405-99(2004)

Standard Practice for Extraction of Tannins from Raw and Spent Materials

$26.00 $52.00

ASTM G103-97(2011)

ASTM G103-97(2011)

Standard Practice for Evaluating Stress-Corrosion Cracking Resistance of Low Copper 7XXX Series Al-Zn-Mg-Cu Alloys in Boiling 6% Sodium Chloride Solution

$25.00 $50.00

ASTM F1357-99(2004)

ASTM F1357-99(2004)

Standard Specification for Articulating Total Wrist Implants

$29.00 $58.00

ASTM D6385-99(2011)

ASTM D6385-99(2011)

Standard Test Method for Determining Acid Extractable Content in Activated Carbon by Ashing

$26.00 $52.00