• ASTM A426/A426M-13

ASTM A426/A426M-13

Standard Specification for Centrifugally Cast Ferritic Alloy Steel Pipe for High-Temperature Service

ASTM International, 11/01/2013

Publisher: ASTM

File Format: PDF

$30.00$60.00


Published:01/11/2013

Pages:5

File Size:1 file , 85 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification2 covers centrifugally cast alloy steel pipe intended for use in high-temperature, high-pressure service.

1.2 Several grades of ferritic steels are covered. Their compositions are given in Table 1.

TABLE 1 Chemical RequirementsA

More ASTM standard pdf

ASTM A1089/A1089M-14

ASTM A1089/A1089M-14

Standard Specification for Highly Loaded Anti-Friction Bearing Steel

$26.00 $52.00

ASTM D4312-95a

ASTM D4312-95a

Standard Test Method for Toluene-Insoluble (TI) Content of Tar and Pitch (Short Method)

$25.00 $50.00

ASTM C1030-95(2001)

ASTM C1030-95(2001)

Standard Test Method for Determination of Plutonium Isotopic Composition by Gamma-Ray Spectrometry

$30.00 $60.00

ASTM F1640-95e1

ASTM F1640-95e1

Standard Guide for Packaging Materials for Foods to Be Irradiated

$27.00 $54.00

Composition, %

Grade

UNS Number

Carbon

Manganese

Phos-
phorus, max

Sulfur, max

Silicon

Chromium

Molybdenum

CP1

J12521

0.25 max

0.30-0.80

0.030

0.025

0.10-0.50

...

0.44-0.65

CP2

J11547

0.10-0.20

0.30-0.61

0.030

0.025

0.10-0.50

0.50-0.81

0.44-0.65

CP5

J42045

0.20 max

0.30-0.70

0.030

0.025

0.75 max

4.00-6.50

0.45-0.65

CP5b

J51545

0.15 max

0.30-0.60

0.030

0.025

1.00-2.00

4.00-6.00

0.45-0.65

CP9

J82090

0.20 max

0.30-0.65

0.030

0.025

0.25-1.00

8.00-10.00

0.90-1.20