• ASTM A588/A588M-04

ASTM A588/A588M-04

Standard Specification for High-Strength Low-Alloy Structural Steel with 50 ksi [345 MPa] Minimum Yield Point to 4-in. [100-mm] Thick

ASTM International, 04/01/2004

Publisher: ASTM

File Format: PDF

$26.00$52.00


Published:01/04/2004

Pages:3

File Size:1 file , 27 KB

Note:This product is unavailable in Russia, Ukraine, Belarus

1.1 This specification covers high-strength low-alloy structural steel shapes, plates, and bars for welded, riveted, or bolted construction but intended primarily for use in welded bridges and buildings where savings in weight or added durability are important. The atmospheric corrosion resistance of this steel in most environments is substantially better than that of carbon structural steels with or without copper addition (see Note 0). When properly exposed to the atmosphere, this steel is suitable for many applications in the bare (unpainted) condition. This specification is limited to material up to 8 in. [200 mm] inclusive in thickness. Note 0For methods of estimating the atmospheric corrosion resistance of low-alloy steels, see Guide G 101.

1.2 When the steel is to be welded, a welding procedure suitable for the grade of steel and intended use or service is to be utilized. See Appendix X3 of Specification A 6/A 6M for information on weldability.

1.3 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system is to be used independently of the other, without combining values in any way.

1.4 The text of this specification contains notes, footnotes, or both, that provide explanatory material. Such notes and footnotes, excluding those in tables and figures, do not contain any mandatory requirements.

1.5 For structural products produced from coil and furnished without heat treatment or with stress relieving only, the additional requirements, including additional testing requirements and the reporting of additional test results, of Specification A 6/A 6M apply.

More ASTM standard pdf

ASTM C973-87(1998)

ASTM C973-87(1998)

Standard Practice for Preparing Test Specimens From Basic Refractory Gunning Products by Pressing

$25.00 $50.00

ASTM C1404/C1404M-98(2003)

ASTM C1404/C1404M-98(2003)

Standard Test Method for Bond Strength of Adhesive Systems Used with Concrete as Measured by Direct Tension (Withdrawn 2010)

$30.00 $60.00

ASTM D3633-98(2006)

ASTM D3633-98(2006)

Standard Test Method for Electrical Resistivity of Membrane-Pavement Systems

$26.00 $52.00

ASTM D5665-99a(2006)

ASTM D5665-99a(2006)

Standard Specification for Thermoplastic Fabrics Used in Cold-Applied Roofing and Waterproofing

$26.00 $52.00