1.1 This specification2 covers precipitation-hardening stainless steel plate, sheet, and strip. The mechanical properties of these steels are developed by suitable low-temperature heat treatments generally referred to as precipitation hardening.
1.2 These steels are used for parts requiring corrosion resistance and high strength at room temperature or at temperatures up to 600°F (315°C). Some of these steels are particularly suitable for moderate to severe drawing and forming in the solution-treated condition. Others are capable of mild forming only. They are suitable for machining in the solution-annealed condition, after which they may be hardened to the mechanical properties specified in this standard without danger of cracking or distortion.
1.3 The values stated in inch-pound units are to be regarded as the standard.
Standard Guide for Conducting Life-Cycle Toxicity Tests with Saltwater Mysids
$38.00 $76.00
Standard Practice for Chemical Protective Clothing Program
$29.00 $58.00
Standard Test Method for Quinoline-Insoluble (QI) Content of Tar and Pitch by Stainless Steel Crucible Filtration
$30.00 $60.00
Standard Specification for Non-Reinforced Extruded Tee Connections for Piping Applications
$32.00 $65.00