1.1 This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS N06625) and nickel-chromium-molybdenum-silicon alloy (UNS N06219)* plate, sheet, and strip.
1.1.1 Alloy UNS N06625 products are furnished in two grades of different heat-treated conditions:
Grade 1 (Annealed)--Material is normally employed in service temperatures up to 1100oF (593oC).
Note 1--Hot-working or reannealing may change properties significantly, depending on working history and temperatures.
1.1.2 Alloy UNS N06219 is supplied in solution annealed condition only.
1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.
Standard Test Method for Determination of Individual Components in Spark Ignition Engine Fuels by 50-Metre Capillary High Resolution Gas Chromatography
$43.00 $86.00
Standard Test Method for Measurement of Creep Crack Growth Times in Metals
Standard Terminology Relating to Electrostatic Discharge (ESD) Packaging Materials
$26.00 $52.00
Standard Test Method for Determination of Dynamic Viscosity and Derived Kinematic Viscosity of Liquids by Constant Pressure Viscometer
$30.00 $60.00