1.1 This test method describes the determination of the total chloride content of polybutenes used for electrical insulation.
1.2 Warning-Mercury has been designated by EPA and many state agencies as a hazardous material that can cause central nervous system, kidney, and liver damage. Mercury, or its vapor, may be hazardous to health and corrosive to materials. Caution should be taken when handling mercury and mercury-containing products. See the applicable product Material Safety Data Sheet (MSDS) for details and EPA's website (http://www.epa.gov/mercury/faq.htm) for additional information. Users should be aware that selling mercury or mercury-containing products, or both, in your state may be prohibited by state law.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. For specific hazards information, see Section 8.
Standard Test Method for Total Ash Content of Activated Carbon
$25.00 $50.00
Standard Specification for Latex Agents for Bonding Fresh To Hardened Concrete
Standard Test Methods for Determination of Iron in Iron Ores and Related Materials by Dichromate Titration
$30.00 $60.00
Standard Specification for Gypsum Lath
$26.00 $52.00